PH13-8Mo Stainless Steel
PH13-8Mo stainless steel is a high-performance material that is martensitic precipitation-hardening stainless steel with about 12-14% chromium, 7-8% nickel, 2-3% molybdenum, and 0.9-1.35% aluminum. It has high strength, excellent fracture toughness, good transverse mechanical properties, and stress corrosion resistance in marine environments, making it suitable for a wide range of applications where high performance and reliability are critical.
PH13-8Mo stainless steel offers stronger mechanical qualities than other iron-based alloys and is ideal for severe conditions. In general, the corrosion resistance of PH13-8Mo steel is superior to that of 1Cr13 and 1Cr17Ni2 (431) martensitic stainless steels; pitting corrosion resistance is superior to that of 17-4 and 15-5 steels due to the addition of molybdenum. It possesses the best corrosion resistance in the fully hardened stage, as do other precipitation-hardening stainless steels. Although PH13-8Mo steel is moderately sensitive to hydrogen embrittlement when aged at temperatures below 565 °C under harsh test conditions, hydrogen embrittlement fracture accidents are uncommon in practical usage. Temperatures above 595 °C protect against hydrogen-induced cracking. Also, this steel has the highest resistance to sulfide stress corrosion cracking when aged at or above 595 °C.
Chemical Composition (%) of PH13-8Mo Stainless Steel
| CHEMICAL COMPOSITION (%) | ||||||||||
| C, max | Mn, max | P, max | S, max | Si, max | Cr | Ni | Mo | N, max | Ti, max | Al |
| 0.05 | 0.10 | 0.010 | 0.008 | 0.10 | 12.25-13.25 | 7.50-8.50 | 2.00-2.50 | 0.010 | 0.10 | 0.80-1.35 |
Mechanical Properties of PH13-8Mo Stainless Steel
| MECHANICAL PROPERTIES | ||||
| Tensile Strength, MPa, min | Yield Strength, MPa, min | Elongation (%), min | Hardness, max | |
| 1210 | 1140 | 12 | 480 HB | 51 HRC |
Physical Properties of PH13-8Mo Stainless Steel
| PHYSICAL PROPERTIES | ||||||
| Density | Modulus of Elasticity | Poisson's Ratio | Coefficient of Thermal Expansion | Thermal Conductivity | Electrical Conductivity | Electrical Resistivity |
| 7.8 g/cm³ | 200 GPa | 0.28 | 11 µm/m·K | 15 W/m·K | 2.3% IACS | 0.7 Ωmm²/m |
Features of PH13-8Mo Stainless Steel
- High strength
- Excellent fracture toughness
- Good transverse mechanical properties
- Good stress corrosion resistance in marine environments
Applications of PH13-8Mo Stainless Steel
PH13-8Mo stainless steel is widely used in chemical industry, petrochemical industry, aerospace, marine, energy, and other fields.
- Plastic film-forming device
- Aircraft parts
- Machined fasteners
- Nuclear reactor parts
Equivalent Grades of PH13-8Mo Stainless Steel
| Grade | ASTM | UNS | WERKSTOFF NR. | GB | EN |
| PH13-8Mo | XM-13 | S13800 | 1.4534 | 04Cr13Ni8Mo2Al | X3CrNiMoAl13-8-2 |
Corrosion Resistance of PH13-8Mo Stainless Steel
The corrosion resistance of PH13-8Mo stainless steel H950 temper to 5% salt spray is comparable to that of 304 stainless steel. The corrosion resistance of PH13-8Mo stainless steel in strong oxidizing and reducing acids is comparable to that of 304 stainless steel. PH13-8Mo stainless steel, like other precipitation-hardening stainless steels, has the best corrosion resistance when fully hardened, and the greater the aging temperature, the worse the corrosion resistance.
In seawater conditions, the forged and welded states of PH13-8Mo stainless steel exhibit good resistance to stress corrosion cracking. The minimum aging temperature for optimal stress corrosion cracking resistance is 538°C.
Hot Forming of PH13-8Mo Stainless Steel
1170-1205 °C is the ideal forging temperature range for PH13-8Mo stainless steel. A deformation of more than 50% below 1040 °C is required to create a refined grain structure.
Cold Forming of PH13-8Mo Stainless Steel
Stainless steel PH13-8Mo can be cold rolled and cold drawn.